INSTRUCTIONS FOR PREHEATING OF RAW MATERIAL

Author:Haifly Machinery Date:2009-12-31 21:24:05
 
                     
FOLLOW BELOW INSTRUCTIONS FOR PREHEATING OF RAW MATERIAL
                     
1 Take the Specified Raw Material for Preheating        
2 Switch `ON' the Oven.              
3 Place the Raw Material in the Trey.            
4 Set the Temperature & Time as given below.          
5 Take out the Raw Material from Oven after the specified Time      
6 Switch OFF the Oven at the end of its use.          
                     
Sr.No.      Raw  Material  Descraption Specified Temp.    
1 Nylon - 6        60 - 80 Degree C. 3 Hours
2 Nylon - 66       100 - 120 Degree C. 3 Hours
3 Nylon - 6 (Glass Filled 30%)  100 - 120 Degree C. 3 Hours
4 Poly Carbonate (Clear)   100 - 120 Degree C. 3 Hours
5 Poly Carbonate (Black)   100 - 120 Degree C. 3 Hours
6 P.P.C.P. - 30%      60 - 80 Degree C. 1 Hours
7 Acrylic (Clear)     60 - 80 Degree C. 2 Hours
8 P.B.T.       60 - 80 Degree C. 2 Hours
9 P.B.T. (Glass Filled)   100 - 120 Degree C. 3 Hours
10 Delrin         80 - 100 Degree C. 4 Hours
11 ABS         60 - 80 Degree C. 3 Hours